SAW wire/flux combination, high-alloyed, austenitic stainless, cryogenic
Price on request
Prices for this catalogue are not published; every quotation is prepared for the requested quantity and delivery terms.
Chemical composition
- Typical analysis
- wt.-% C Si Mn Cr Ni W
- wire 0.20 0.4 10.2 17.5 14 3.5
- all-weld metal 0.18 0.5 9.3 17.2 14.0 3.4
Mechanical properties
Mechanical properties of all-weld metal – typical values (min. values)
| Condition | Yield strength (MPa) | Tensile strength (MPa) | Elongation (%) | Impact ISO-V (J) | |
|---|---|---|---|---|---|
| +20°C | -196°C | ||||
| u | > 430 | > 620 | > 30 | 80 | 50 |
u untreated, as welded
Current type
DC+ Dimension mm
Documentation
Documents open on the manufacturer's website.