Classification: E Z Fe8 (EN 14700)
Rutile coated electrode for hardfacing of parts, subjected to high metal-to-metal wear, compression and impact at elevated temperatures.
Price and availability are provided by quotation. Send an enquiry with quantity and variant.
Product description
Rutile coated electrode for hardfacing of parts, subjected to high metal-to-metal wear, compression and impact at elevated temperatures. Due to its Cr, Mo and Co alloy content, weld metal has high mechanical strength, toughness and thermal resistance to operating temperatures up to 650° C. Has excellent welding properties, a stable and regular metal drop flow, good weld appearance and very easy slag removal. Typical Applications: Used for hot work tool steels, hot shear blades, forging dies, aluminum casting and extrusion plactic screws.
Standards and classifications
| EN 14700 | E Z Fe8 |
| TS EN 14700 | E Z Fe8 |
| DIN 8555 | E 3-UM-50-GTZ |
Typical chemical values of weld metal
| Type of Analysis | C | Si | Mn | Cr | Mo | Co |
|---|---|---|---|---|---|---|
| Weld Deposit | 0.10 | 0.40 | 0.10 | 10.0 | 3.50 | 14.0 |
Typical mechanical values of weld metal
| Test Condition | Hardness (HRc) |
|---|---|
| As welded | 50 |
Welding positions
Polarity
Welding parameters and efficiency
| Diameter x Length (mm) | Current (A) |
|---|---|
| 2.50x300 | 60-90 |
| 3.25x350 | 90-120 |
| 4.00x350 | 130-160 |
Wear resistance
| Property | Level |
|---|---|
| Abrasion | Medium |
| Adhesion | Very High |
| Impact | Medium |
| Temperature | Very High |
| Corrosion | Medium |
Scale as published in the official Magmaweld chart: Low · Medium · High · Very High
Variants and packaging
| Product Code | Diameter X Length (mm) | Pieces per Box (~) | Weight Of The Box (kg) | Boxes Per Package | Weight Of The Package | Packaging Type |
|---|---|---|---|---|---|---|
| 18025GDEM2 | 2.50x300 | 127 | 2.5 | 3 | 8.1 | Plastic Box |
| 18025NDEM2 | 3.25x350 | 67 | 2.5 | 3 | 8.1 | Plastic Box |
| 18025QDEM2 | 4.00x350 | 42 | 2.5 | 3 | 8.1 | Plastic Box |
Storage and re-drying
- It can be dried maximum 5 times.
- Generally not required. If required, redry for 2 hour at 150°C.
Documentation