Classification: E308Mo-15 (AWS/ASME SFA - 5.4)
Basic electrode, particularly designed for welding armour plates, dissimilar steels and for surfacing purposes.
Price and availability are provided by quotation. Send an enquiry with quantity and variant.
Product description
Basic electrode, particularly designed for welding armour plates, dissimilar steels and for surfacing purposes. The weld metal consists of austenitic Cr-Ni-Mn-Mo stainless steel. It features high resistance to cracking caused by impact and high temperature and is therefore indicated for difficult to weld steels and depositing stress relaxing buffer layers on crack sensitive base metal or beneath hardfacing deposits. Use with DCEP. No pre-heat or post welding heat treatment is needed when welding armour plates. Interpass temperature should not exceed 120°C. Shall be used with shortest possible stick-out distance, at 90° angle to the work piece.
Standards and classifications
| AWS/ASME SFA - 5.4 | E308Mo-15 |
| EN ISO 3581 - A | E 20 10 3 B 22 |
| TS EN ISO 3581 - A | E 20 10 3 B 22 |
| DIN M. No. | 1.4443 |
Typical chemical values of weld metal
| Type of Analysis | C | Si | Mn | Cr | Ni | Mo |
|---|---|---|---|---|---|---|
| Weld Deposit | 0.08 | 0.55 | 1.80 | 20.00 | 11.50 | 2.50 |
Typical mechanical values of weld metal
| Test Condition | Yield Strength (N/mm²) | Tensile Strength (N/mm²) | Elongation A5 (%) | Charpy V-Notch Properties (J) |
|---|---|---|---|---|
| As welded | 440 | 690 | 40 | 20°C → 70 |
Welding positions
Polarity
Welding parameters and efficiency
| Diameter x Length (mm) | Current (A) |
|---|---|
| 2.50x250 | 50-80 |
| 2.50x300 | 50-80 |
| 3.25x300 | 80-120 |
| 3.25x350 | 80-120 |
| 4.00x350 | 100-165 |
| 5.00x350 | 140-220 |
Variants and packaging
| Product Code | Diameter X Length (mm) | Pieces per Box (~) | Weight Of The Box (kg) | Boxes Per Package | Weight Of The Package | Packaging Type |
|---|---|---|---|---|---|---|
| 13007GJEM2 | 2.50x300 | 104 | 1.8 | 10 | 18.5 | VAC Box |
| 13007MJEM2 | 3.25x300 | 62 | 1.8 | 10 | 16.3 | VAC Box |
| 13007NJEM2 | 3.25x350 | 60 | 2.0 | 10 | 0.0 | VAC Box |
| 13007QJEM2 | 4.00x350 | 46 | 2.0 | 9 | 18.6 | VAC Box |
| 13007TJEM2 | 5.00x350 | 25 | 2.0 | 9 | 18.8 | VAC Box |
Storage and re-drying
- It can be dried maximum 5 times.
- It has to be dried at 350°C for 2 hours.