Classification: E316L-15 (AWS/ASME SFA - 5.4)
Basic type stainless steel electrode for welding austenitic stainless Cr-Ni-Mo steels and cast steels, having a low carbon content.
Price on request
Price and availability are provided by quotation. Send an enquiry with quantity and variant.
Product description
Basic type stainless steel electrode for welding austenitic stainless Cr-Ni-Mo steels and cast steels, having a low carbon content. For operating temperatures up to 400°C. Especially suitable for welding of stainless steel chemical tanks and pipes made of low carbon austenitic 19Cr/12Ni/2-3Mo stainless steels in chemical, textile, paint, paper industries. Used with DCEP.
Standards and classifications
| AWS/ASME SFA - 5.4 | E316L-15 |
| EN ISO 3581 - A | E 19 12 3 L B 42 |
| TS EN ISO 3581 - A | E 19 12 3 L B 42 |
| DIN M. No. | 1.4430 |
Base materials
| EN | Material | ASTM |
|---|---|---|
| X3CrNiMo17-13-3 | 1.4436 | 316 |
| X5CrNiMo17-12-2 | 1.4401 | 316 |
| GX2CrNiMo19-11-2 | 1.4409 | |
| X2CrNiMo17-12-2 | 1.4404 | 316L |
| GX5CrNiMo19-11-2 | 1.4408 | CF-8M |
| X2CrNiMo18-14-3 | 1.4435 | 316L |
| X6CrNiMoTi17-12-2 | 1.4571 | 316 Ti |
| X6CrNiMoNb17-12-28 | 1.4580 | 316 Cb |
| G-X5CrNiMoNb19-11-2 | 1.4581 | |
| 1.4583 | 318 | |
| X10CrNiMo18-12 | 1.4583 |
Typical chemical values of weld metal
| Type of Analysis | C | Si | Mn | Cr | Ni | Mo |
|---|---|---|---|---|---|---|
| Weld Deposit | 0.02 | 0,50 | 0.80 | 18.00 | 13.00 | 2.80 |
Typical mechanical values of weld metal
| Test Condition | Yield Strength (N/mm²) | Tensile Strength (N/mm²) | Elongation A5 (%) | Charpy V-Notch Properties (J) |
|---|---|---|---|---|
| As welded | 480 | 590 | 38 | 20°C → > 70 |
Welding positions
PAPBPCPDPEPF
Polarity
DC(+)
Welding parameters and efficiency
| Diameter x Length (mm) | Current (A) |
|---|---|
| 2.50x300 | 55-75 |
| 3.25x350 | 70-120 |
| 4.00x350 | 100-165 |
Variants and packaging
| Product Code | Diameter X Length (mm) | Pieces per Box (~) | Weight Of The Box (kg) | Boxes Per Package | Weight Of The Package | Packaging Type |
|---|---|---|---|---|---|---|
| 13018GJEM2 | 2.50x300 | 96 | 1.8 | 10 | 16.3 | VAC Box |
| 13018NJEM2 | 3.25x350 | 57 | 2.0 | 10 | 18.6 | VAC Box |
| 13018QJEM2 | 4.00x350 | 37 | 2.0 | 10 | 18.6 | VAC Box |
Storage and re-drying
- It can be dried maximum 5 times.
- It has to be dried at 350°C for 2 hours.